Polymer Property : Tensile Modulus = 8.29 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 8.29 GPa
1200 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12 (Asia Pacific)
LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System.
Tensile Modulus 8.29 GPa
1200 ksi
1mm/min; ISO 527
BASF Ultramid® SEGM35 H1 BK-126 15/25% Glass/Mineral Filled PA6 (Dry)
Ultramid SEGM35 H1 BK-126 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compared to 8267G ..
Tensile Modulus 8.29 GPa
1200 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12
LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System.