Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.26 GPa | 1200 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DX10311 PC (Asia Pacific) DX10311 is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility. |
|||
Tensile Modulus | 8.26 GPa | 1200 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP BF004 SAN LNP* THERMOCOMP* BF004 is a compound based on SAN resin containing 20% Glass Fiber. |