Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.68 GPa | 1110 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC LNP* STAT-KON* DX05474 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Retardant, Mold .. |
|||
Tensile Modulus | 7.68 GPa | 1110 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC (Asia Pacific) LNP* Stat-kon* DX05474 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Ret.. |