Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.61 GPa | 1100 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3240A PP SABIC® PPcompound G3240A is a general purpose, 40% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 139448304. |
|||
Tensile Modulus | 7.61 GPa | 1100 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3240U PP SABIC® PPcompound G3240U is a general purpose, 40% glass filled, chemically coupled, heat stabilized and UV stabilized homopolymer polypropylene compound. The IMDS ID is 209768078. |
|||
Tensile Modulus | 7.61 GPa | 1100 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP JF004P PES (Asia Pacific) LNP* Thermocomp* JF004P is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Exceptional Processing. |
|||
Tensile Modulus | 7.61 GPa | 1100 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP JF004P PES LNP* THERMOCOMP* JF004P is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Exceptional Processing. |