Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.38 GPa | 1070 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF0049E PC (Asia Pacific) LNP* Thermocomp* DF0049E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Easy Molding, Flame Retardant. |
|||
Tensile Modulus | 7.38 GPa | 1070 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS LNP* STAT-KON* AE002 is a compound based on ABS resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 7.38 GPa | 1070 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF0049E PC LNP* Thermocomp* DF0049E is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Flame Retardant. |
|||
Tensile Modulus | 7.38 GPa | 1070 ksi | ASTM D638 |
LNP Thermocomp® HF-1006 Polyamide 11, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |