Polymer Property : Tensile Modulus = 7.25 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.0500 GPa
7.25 ksi
ISO 527-1/-2
DSM Arnitel® EM402-L Polyether Ester Elastomer (European Grade)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.0500 GPa
7.25 ksi
ISO 527-1/-2
DSM Arnitel® EM400 40 Shore D, Injection or Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.0500 GPa
7.25 ksi
ISO 527-1/-2
DSM Arnitel® EM400 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.0500 GPa
7.25 ksi
ISO 527-1/-2
DSM Arnitel® EM400-BP TPC-ET
34 Shore D, Injection Molding or Extrusion Grade
Tensile Modulus 0.0500 GPa
7.25 ksi
1 mm/min
Arkema Group Evatane® 1003 VL 4S Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Grade for transparent and thermal agricultural film to 180 at 200 µ for greenhouse coverage.ISO data prov..
Tensile Modulus 0.0500 GPa
7.25 ksi
1 mm/min
Arkema Group Evatane® 1005 VN 5 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for films with high transparency and high mechanical properties. Examples: coextrusion, stretch film, paper-stationary, fancy ..
Tensile Modulus 0.0500 GPa
7.25 ksi
1 mm/min
Arkema Group Evatane® 1020 VN 5 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for molding flexible articles. Examples: fittings, rail pads, medical.ISO data provided by the manufacturer, Arkema.
Tensile Modulus 0.0500 GPa
7.25 ksi
1 mm/min
Arkema Group Evatane® 1080 VN 5 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for molding very flexible articles. Examples: gaskets, medical.ISO data provided by the manufacturer, Arkema.
Tensile Modulus 0.0500 GPa
7.25 ksi
average; in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® R63.80 Damage Tolerant Foam
AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable..
Tensile Modulus >= 0.0500 GPa
>= 7.25 ksi
in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® R82.80 High Performance Structural Foam
AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver..
Tensile Modulus 0.0500 GPa
7.25 ksi
1 mm/min
Arkema Group Evatane® 1020 VG 5 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for flexible films with high mechanical properties. Examples: films, chemical bags, gloves.ISO data provided by the manufactur..
Tensile Modulus 0.0500 GPa
7.25 ksi
ISO 527-1/-2
DSM Arnitel® EM402-L Injection Molding; Coating Grade Copolyester Elastomer (North America)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus >= 0.0500 GPa
>= 7.25 ksi
in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® C70.75 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..