Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.17 GPa | 1040 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Tensile Modulus | 7.17 GPa | 1040 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive. Wear Resistant, Flame Retardant. |
|||
Tensile Modulus | 7.17 GPa | 1040 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC (Asia Pacific) LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 7.17 GPa | 1040 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF004 PA 66 LNP THERMOCOMP* RF004 is a compound based on Nylon 66 resin containing 20% Glass Fiber. |
|||
Tensile Modulus | 7.17 GPa | 1040 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF004H PA 66 LNP* THERMOCOMP* RF004H is a compound based on Nylon 66 containing 20% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Tensile Modulus | 7.17 GPa | 1040 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXD PA 66 LNP THERMOCOMP* RF004XXD is a compound based on Nylon 66 resin containing 20% Glass Fiber. |
|||
Tensile Modulus | 7.17 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL FE1520PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1520PW resin is a blend of polyphenylene oxide (PPO) and polystyrene (PS) resin that contains 20% glass reinforcement. The resin is suitable for injection molding. Noryl FE1520PW resin has .. |
|||
Tensile Modulus | 7.17 GPa | 1040 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC (Asia Pacific) LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup.. |