Mechanical Properties Metric English Comments
Tensile Modulus 0.451 GPa
65.4 ksi
ASTM D638
Daikin NEOFLON AP-210AS PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for injection molding.Information provided by D..
Tensile Modulus 0.451 GPa
65.4 ksi
ASTM D638
Daikin NEOFLON AP-230ASL PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for extrusion molded parts. Piping, tube, etc...
Tensile Modulus 0.451 GPa
65.4 ksi
ASTM D638
Daikin NEOFLON AP-201 PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Complicated injection molded parts requiring high melt flow to fil..
Tensile Modulus 0.451 GPa
65.4 ksi
ASTM D638
Daikin NEOFLON AP-210 PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Injection molded parts, wire insulation, etc.Information provided ..
Tensile Modulus 0.451 GPa
65.4 ksi
ASTM D638
Daikin NEOFLON AP-230 PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Linings, tubing, etc.Information provided by Daikin Industries.