Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.37 GPa | 634 ksi | same value from ASTM and ISO test. |
BASF Capron® 8331G HS Blend Impact Modified, 14% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8331G HS Blend is a 14% glass fiber reinforced, heat stabilized, polyamide 6 molding compound developed for applications requiring improved toughness in combination with a balance of strength.. |