Mechanical Properties Metric English Comments
Tensile Modulus 6.48 GPa
940 ksi
ASTM D638
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
Tensile Modulus 6.48 GPa
940 ksi
ASTM D638
Quadrant EPP Semitron® 480 ESd PEEK, static dissipative, extruded (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic ProductsThis PEEK based static dissipative material provides a dissipative range of 10E+6 - 10E+9 ohms/sq. Semitron® ESd 480 is very dimensionally sta..
Tensile Modulus 6.48 GPa
940 ksi
ASTM D638
Quadrant EPP Semitron® ESd 490HR Static dissipative PEEK for use in test fixtures. Non-sloughing and low moisture absorption. (ASTM Product Data Sheet)
Tensile Modulus 6.48 GPa
940 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM 2312EPR PEI
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Tensile Modulus 6.48 GPa
940 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM 2312EPR PEI (Asia Pacific)
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Tensile Modulus 6.48 GPa
940 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East)
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
Tensile Modulus 6.48 GPa
940 ksi
ASTM D638
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry)
Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
Tensile Modulus 6.48 GPa
940 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DX06410 PC (Asia Pacific)
LNP* Thermocomp* DX06410 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Tensile Modulus 6.48 GPa
940 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS
LNP* THERMOCOMP* NF004 is a compound based on PC+ABS resin containing 20% Glass Fiber.
Tensile Modulus 6.48 GPa
940 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS (Asia Pacific)
LNP* Thermocomp* NF004 is a compound based on PC+ABS Blend resin containing Glass Fiber.
Tensile Modulus 6.48 GPa
940 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DX06410 PC
LNP* THERMOCOMP* DX06410 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.