Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.41 GPa | 930 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C4220 PC+ABS PC+ABS Blend with 20% Glass Reinforce. High heat resistance; Excellent balance strength/rigidity; Good impact/appearance. |
|||
Tensile Modulus | 6.41 GPa | 930 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP JF003XXZ PES LNP* THERMOCOMP* JF003XXZ is a compound based on Polyethersulfone resin containing 15% Glass Fiber. |
|||
Tensile Modulus | 6.41 GPa | 930 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP JF003XXZ PES (Asia Pacific) LNP* Thermocomp* JF003XXZ is a compound based on Polyethersulfone resin containing Glass Fiber. |
|||
Tensile Modulus | 6.41 GPa | 930 ksi | ASTM D638 |
Ensinger Tecapeek® XP-105 Compression Molded PEEK Compound, 15% Graphite Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Modulus | 6.41 GPa @Temperature 150 °C |
930 ksi @Temperature 302 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **) Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg.. |