Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 56.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON F-104 PTFE Fine Powder
Processing Methods: Paste extrusion, calendering.Applications: Unsintered tape, sealing tape, low specific gravity tape, tape for wrapping flat cables, tubes.Information provided by Daikin Industrie..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON F-201 PTFE Fine Powder
Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries.
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON F-205 PTFE Fine Powder
Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries.
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON F-302 PTFE Fine Powder
Processing Methods: Paste extrusion.Applications: Small to large diameter tubes, flexible hoses, shrinkable tubes, heavy duty electric wires smaller than AGW18, and jackets.Information provided by ..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON M-111 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with extremely smooth and fine surface. Suited to making packing and gaskets since moldings have an especially go..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON M-112 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with especially good elasticity, making it ideal for molding diaphragms and bellows. Offers excellent post-moldin..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON M-12 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Useful in making products requiring fine texture, especially insulation skiving tapes. Also allows uniform mixing of inorganic fill..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON M-139 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding and automatic compression molding.Features: Excellent fluidity. Apparent density is large and ideal for automated compression molding proces..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON M-18 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Suited to molding of large billets, has nearly the same molding characteristics of M-12. Also allows uniform mixing of inorganic fi..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON M-391 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding and automatic or semi-automatic compression molding.Features: Used if concerned about insufficient molding pressure for flat sheets.Informati..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON M-392 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding, automatic or semi-automatic compression molding, isostatic molding, and ram extrusion.Features: Good fill characteristics particularly into ..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON M-393 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding, automatic compression molding, and ram extrusion.Features: Maximum emphasis given to ease of handling during molding. Used when molded arti..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON MG-1030 PTFE 15% Glass Fiber Filled Molding Powder
15% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON MG-1040 PTFE 20% Glass Fiber Filled Molding Powder
20% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON MG-1040F PTFE 20% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow
20% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON MG-1050F PTFE 25% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow
25% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON MG-1241 PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder
20% glass fiber and 5% graphite filled. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (e.g. piston rings, bearing pads, and packings)Inform..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON MG-1241F PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder, High Apparent Density, Free Flow
20% glass fiber and 5% graphite filled. High apparent density and free-flowing properties. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON MG-1431 PTFE 15% Glass Fiber and 5% MoS2 Filled Molding Powder
15% glass fiber and 5% MoS2 filled. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanical and electrical service (e.g. split-curled bearings..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON MG-1431F PTFE 20% Glass Fiber and 5% MoS2 Filled Molding Powder, High Apparent Density, Free Flow
15% glass fiber and 5% MoS2 filled. High apparent density and free-flowing properties. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanica..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON MG-2030 PTFE 15% Graphite Filled Molding Powder
15% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON MG-2060 PTFE 30% Graphite Filled Molding Powder
30% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON MG-6030 PTFE 15% Carbon Fiber Filled Molding Powder
15% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by ..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON MG-6030F PTFE 15% Carbon Fiber Filled Molding Powder, High Apparent Density, Free Flow
15% carbon fiber filled. High apparent density and free-flowing properties. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechan..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON MG-6050 PTFE 25% Carbon Fiber Filled Molding Powder
25% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by ..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON MG-1030F PTFE 15% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow
15% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl..
Tensile Modulus 0.392 GPa
56.9 ksi
ASTM D638
Daikin POLYFLON MG-1050 PTFE 25% Glass Fiber Filled Molding Powder
25% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,..
Copyright © lookpolymers.com All Rights Reserved