Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.65 GPa @Temperature 22.8 °C |
530 ksi @Temperature 73.0 °F |
ASTM D638 |
Quadrant EPP Ketron® CM HPV PEEK (1331) Compression Molded High Pressure Velocity Polyetherether Ketone |
|||
Tensile Modulus | 3.65 GPa | 530 ksi | ASTM D638 |
Quadrant EPP Ketron® CM HPV PEEK Polyetheretherketone; PTFE, Graphite, and Carbon Fiber Filled Bearing Grade, compression molded (ASTM Product Data Sheet) Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam |
|||
Tensile Modulus | 3.65 GPa | 530 ksi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4731-13 Polycarbonate EMERGEâ„¢ PC 4731-13 advanced resin is formulated with 10% glass fiber and has an f1 rating by Underwriters Laboratories Inc. It provides good ignition resistance, rigidity, dimension stability .. |
|||
Tensile Modulus | 3.65 GPa | 530 ksi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4731-8 Polycarbonate EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 10% glass fiber and has an f1 rating by Underwriters Laboratories Inc. It provides good ignition resistance, rigidity, dimension stability .. |
|||
Tensile Modulus | 3.65 GPa | 530 ksi | ASTM D638 |
Styron EMERGEâ„¢ 4701-13 Polycarbonate EMERGEâ„¢ PC 4701-13 advanced resin is formulated with 10% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
Tensile Modulus | 3.65 GPa | 530 ksi | ASTM D638 |
Lubrizol ESTALOC® 59300 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro.. |