Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.61 GPa | 524 ksi | ASTM D882 |
NatureWorks® Ingeo™ 2003D General Purpose Transparent Extrusion Grade Biopolymer NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. PLA polymer 2003D processes easily on conventional extrusion equipment. Specifically designed fo.. |
|||
Tensile Modulus | 3.61 GPa | 524 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MX88028 PP LNP* THERMOCOMP* MX88028 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Tensile Modulus | 3.61 GPa | 524 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MX88028 PP (Asia Pacific) LNP* Thermocomp* MX88028 is a compound based on Polypropylene resin containing Glass Fiber. |