Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 52.2 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.360 - 0.480 GPa

@Thickness 2.00 mm
52.2 - 69.6 ksi

@Thickness 0.0787 in
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)
Solef® 21510 PVDF copolymer has medium viscosity and is suitable for extrusion and for solution processing in lithium batteries applications.Features: Copolymer; Good Flexibility; Medium Viscosit..
Tensile Modulus 0.360 GPa
52.2 ksi
ISO 527-1/-2
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P40 Nylon, conditioned
Hiprolon® 11ESNNHL P40 long chain polyamide compound contains a bio-renewable resource. It features low density, low water absorbing, high dimension stability and heat stability, high cold impact..
Tensile Modulus 0.360 GPa
52.2 ksi
cond; ISO 527-1/-2
DSM Novamid® ST145 NAT PA6-I
Impact Modified, Injection Molding
Tensile Modulus 0.360 GPa
52.2 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® L 25 W 40 X PA12-I
Product Description: Grilamid L 25 W 40 X is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 X is impact modified and heat and UV stabilized. The m..
Tensile Modulus 0.360 GPa
52.2 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® L 22A W 40 X PA12-I
Product Description: Grilamid L 22A W 40 X is a flexible plasticized and impact modified heat and light stabilized Polyamide 12 (PA12). The main features of Grilamid L 22A W 40 X are: Good impact st..
Tensile Modulus 0.360 GPa
52.2 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® L 25 W 40 HL X PA12-I
Product Description: Grilamid L 25 W 40 HLX is a flexible Polyamide 12 grade with an excellent cold impact strength and heat stability. Grilamid L 25 W 40 HLX is specially suitable for flexible tube..
Tensile Modulus 0.360 GPa

@Temperature 110 °C
52.2 ksi

@Temperature 230 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66  (Unverified Data**)
Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers
Tensile Modulus 0.360 GPa

@Temperature 120 °C
52.2 ksi

@Temperature 248 °F
ISO Data
BASF Ultramid® 8202 HS PA6 (Dry)
Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab..
Tensile Modulus 0.360 GPa

@Temperature 120 °C
52.2 ksi

@Temperature 248 °F
ISO Data
BASF Ultramid® 8202 PA6 (Dry)
Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult..
Tensile Modulus 0.360 - 0.480 GPa

@Thickness 2.00 mm,
Temperature 23.0 °C
52.2 - 69.6 ksi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type IV, 1.0 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 21510 PVDF copolymer has low viscosity and is suitable for solution processing in lithium batteries applications.Information provided by Solvay Specialty Polymers.
Copyright © lookpolymers.com All Rights Reserved