Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.93 GPa @Temperature 150 °C |
860 ksi @Temperature 302 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Tensile Modulus | 5.93 GPa @Temperature 150 °C |
860 ksi @Temperature 302 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Tensile Modulus | 5.93 GPa | 860 ksi | ASTM D638 |
Westlake Plastics Zelux® 20% GF Polycarbonate 20% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Tensile Modulus | 5.93 GPa | 860 ksi | ASTM D638 |
Ensinger Tecanat™ GF20 20% Glass Reinforced Polycarbonate (PC) Tenacat™ GF20 is typically used in business equipment where gears, rollers, interlam mechanical parts, connectors and relays are required. The automotive industry uses polycarbonate materials for .. |
|||
Tensile Modulus | 5.93 GPa | 860 ksi | ASTM D638 |
Quantum Polycarbonate 20% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Tensile Modulus | 5.93 GPa | 860 ksi | ASTM D638 |
Oxford Polymers 20GF 20% Glass Fiber Filled Polycarbonate for Injection Molding 20% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Tensile Modulus | 5.93 GPa | 860 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AX06472 ABS LNP* Thermocomp* AX06472 is a compound based on ABS containing a clay blend. |