Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.83 GPa | 846 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp MX88073 PP (Asia Pacific) LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 5.83 GPa | 846 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp MX88073 PP LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 5.83 GPa | 846 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOTUF PX95726 PA 6 LNP THERMOTUF* PX95726 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |