Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.80 GPa | 841 ksi | |
Plastcom SLOVAMID 6 GF 10 FRC 2 PA6, 10% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically strengthened with 10 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | |
Plastcom SLOVAMID 66 GF 15 T 6 TS PA66, 15% glass fibre, 6% talc FeaturesChemically reinforced with 15% glass fibre and 6% of talc, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrica.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | |
Plastcom SLOVAMID 66 T 40 FRO 3 PA66, 40% mineral filling, flame retardant FeaturesPA 66 with the content of 40% chemically modified mineral filling a with fire retardant. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat produ.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CM4219 PC+ABS (Asia Pacific) |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ASTM D638 |
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | |
Plastcom SLOVAMID 6 GF 10 GB 20 PA6, 10% glass fibre, 20% glass beads FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre and 20% glass beads. Application: impacted mouldings and mouldings with high strength applied in automotive, electri.. |
|||
Tensile Modulus | 5.80 GPa @Temperature 175 °C |
841 ksi @Temperature 347 °F |
ISO 527 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ISO 527 |
Victrex® APTIV® 1103-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, Mineral Filled
(Unve Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ISO 527-1,-2 |
Lanxess Durethan® BM 240 H3.0 000000 Nylon 6, 40% Mineral PA 6, 40% mineral, injection molding, heat-ageing stabilized, low tendency to warp, isotopic properties |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 (Asia Pacific) LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF VF004S SUPER TOUGH NYLON (Europe-Africa-Middle East) LNP* THERMOTUF* VF004S is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Asia Pacific) Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 1013G15 1 NA PA6-GF15 15% Glass Reinforced, Injection Molding |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® B 70 GFE 30 H PA6-GF30 Product description: Grilon B 70 GFE 30 H is a heat stabilized and impact modified PA 6 injection molding grade with 30% glass fiber reinforcement. Grilon B 70 GFE 30 H has the following important p.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGZ-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® 11C140 BK086 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66 Minlon 11C140 BK086 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding. It has very low warpage.Information provided by Du.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66 Minlon 11C40 BKB086 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK416 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 resin for injection molding.Information provided by.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide BK8 PA6, 40% Mineral Fiber Filled, Injection Molded Staramide BK8 is a 40% Mineral Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam BFR552Y3 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR552Y3 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ISO 527 |
Eurostar Starglas FF006 HDPE, Glass Fiber Filled Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene Resin (also known as Starglas PE HE 30V)Information provided by Eurostar. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | Transverse direction; ISO 527/4 |
Azdel Plus U400-B01N 41.5% Directionalized Continuous Fiber Mat / PP Resin Matrix AZDEL® U400-B01N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. Thi.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity. |