Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.77 GPa | 837 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® MC5215 PC+ABS |
|||
Tensile Modulus | 5.77 GPa | 837 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® MC5215 PC+ABS (Asia Pacific) |
|||
Tensile Modulus | 5.77 GPa | 837 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP HH0420A PA11 LNP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
Tensile Modulus | 5.77 GPa | 837 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP HH0420A PA11 LNP* THERMOCOMP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
Tensile Modulus | 5.77 GPa | 837 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON NV003E PC+ABS (Asia Pacific) LNP* Verton* NV003E is a compound based on PC+ABS Blend resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Tensile Modulus | 5.77 GPa | 837 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON NV003E PC+ABS LNP* VERTON* NV003E is a compound based on PC+ABS Blend resin containing 15% Long Glass Fiber. Added features of this material include: Easy Molding, Structural. |