Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.6857 GPa | 824.64 ksi | Storage |
Epoxy Technology EPO-TEK® H31 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H31 is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electronic.. |