Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.67 GPa | 822 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AF003 ABS (Asia Pacific) LNP* Thermocomp* AF003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. |
|||
Tensile Modulus | 5.67 GPa | 822 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 2F005 ETFE LNP* Thermocomp* 2F005 is a fluoropolymer compound based on ETFE containing 25% Glass Fiber. |