Polymer Property : Tensile Modulus = 5.24 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 5.24 GPa
760 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM 2110EPR PEI
10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.
Tensile Modulus 5.24 GPa
760 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM 2110EPR PEI (Asia Pacific)
10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.
Tensile Modulus 5.24 GPa
760 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON MX01739C PP
LNP* SAT-KON* MX01739C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System.
Tensile Modulus 5.24 GPa
760 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RZ0069 PA 66 (Asia Pacific)
LNP* Thermocomp* RZ0069 is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant, Milled Glass. Added features of this material include: Flame Retardant.
Tensile Modulus 5.24 GPa
760 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF002 PA 66
LNP THERMOCOMP* RF002 is a compound based on Nylon 66 resin containing 10% Glass Fiber.
Tensile Modulus 5.24 GPa
760 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RZ0069 PA 66
LNP* THERMOCOMP* RZ0069 is a compound based on Nylon 66 resin containing 30% Milled Glass. Added features of this material include: Flame Retardant.
Tensile Modulus 5.24 GPa
760 ksi
ASTM D638
Asahi Kasei Thermylene® P6-30FG-0699 30% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Tensile Modulus 5.24 GPa
760 ksi
ASTM D638
Asahi Kasei Thermylene® P6-30FG-0155 30% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Tensile Modulus 5.24 GPa
760 ksi
ASTM D638
Asahi Kasei Thermylene® P6-30FG-0687 30% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil