Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 33.0 GPa | 4790 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON E9007E PEI LNP* VERTON* E9007E is a compound based on Polyetherimide (PEI) containing 35% Long Carbon Fiber. Added features of this grade include: Structural, High Temperature |
|||
Tensile Modulus | 33.0 GPa | 4790 ksi | Results normalized to 60% fibre volume for Carbon, 50% fibre volume for Kevlar; pr EN 2561 Type B |
Hexcel® HexPly® 920KX-285-52% 125°C Curing Epoxy Matrix Kevlar, 4H satin, 171 g/m2Information provided by HexCel |