Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.25 GPa | 471 ksi | |
Plastcom SLOVALEN PH 99 GB 30 LS PP, 30% glass beads, mod. of mech. properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | Type 1B, 50mm/min; ISO 527-1/2:1993 |
Nylacast Impact Nylon 6, Impact Grade Nylacast Impact has been designed for applications that have a high impact resistance and noise reduction capabilities. It works more effectively in applications where there are high stress. It also.. |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | 1 mm/min; ISO 527 |
Polimeri Europa Edistir N 1782 Polystyrene General purpose polystyrene with good flow and high heat resistance. Suggested for direct gassing extrusion of heavy gage insulating boards (XPS) and in blend with high concentration of clear SBS f.. |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | 1 mm/min; ISO 527 |
Polimeri Europa Edistir N 1840 Polystyrene General purpose polystyrene combining easy flow and medium heat. Edistir N 1840 is suggested in extrusion for glossy capping of HIPS sheets and for blending with HIPS or clear SBS for stiffer therm.. |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | 1 mm/min; ISO 527 |
Polimeri Europa Edistir N 2560 Polystyrene High molecular weight general purpose polystyrene with good mechanical strength and good thermal resistance. It is recommended for in-line forming of disposable packaging, for sheet
extrusion in ble.. |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | ISO 527-1/2 |
Radici Radilon® ALX14080 (dry) Nylon 66 Medium high viscosityInformation provided by Radici group. |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | 1 mm/min |
Polimeri Europa EDISTIR N1460 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,E,085-03 High molecular weight general purpose polystyrene with good mechanical strength. This grade is especially recomme.. |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | 1 mm/min |
Polimeri Europa EDISTIR N1461 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,085-03 High molecular weight general purpose polystyrene with good mechanical strength. Well suitable for injection mold.. |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | 1 mm/min |
Polimeri Europa EDISTIR N1841 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,085-12 General purpose polystyrene combining easy flow and medium heat. This grade exhibits excellent processability in .. |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | ISO 527 |
FKuR Kunststoff Fibrolon® P 7550 Wood-Plastic Compound, Fiber Reinforced FIBROLON® are fiber reinforced compounds. Fibrolon® P 7550 has a polypropylene base. With the brand name of FIBROLON® FKuR has developed natural fiber reinforced compounds (Wood-Plastics-C.. |
|||
Tensile Modulus | 3.25 GPa @Temperature 80.0 °C |
471 ksi @Temperature 176 °F |
1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC STAMAX 20YK270 PP SABIC® STAMAX 20YK270 is a 20% long glass fiber reinforced polypropylene with improved impact and flow properties. The glass fibers are chemically coupled to the PP matrix, resulting in high stif.. |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP EX00781H PEI LNP* THERMOCOMP* EX00781H is a compoud based on Polyetherimide containng Proprietary Filler(s). Added feature of this material is: Healthcare. |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MFB22S PP LNP* THERMOCOMP* MFB22S is a compound based on Polypropylene containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Heat Stabilized. |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 Conductive GTX, CTE 7 |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 (Asia Pacific) Conductive GTX, CTE 7 |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 (Europe-Africa-Middle East) Conductive GTX, CTE 7 |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP LNP THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 3.25 GPa @Temperature 22.8 °C |
471 ksi @Temperature 73.0 °F |
ASTM D638 |
Ensinger TECANYL™ MT Autoclavable Polymer TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease.. |
|||
Tensile Modulus | 3.25 GPa @Temperature 22.8 °C |
471 ksi @Temperature 73.0 °F |
ASTM D638 |
Ensinger TECANYL™ MT XRO Autoclavable Polymer TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease.. |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | ISO 527 |
Eurotec® Tecomid® NA40 MR15 NL IL PA6.6, 15% mineral filled, impact modified, natural Information provided by Eurotec® |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | ISO 527 |
Eurotec® Tecomid® NB40 NL FY70 PA6, flame retardant - halogen free (RoHS compliant), natural Information provided by Eurotec® |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | ISO 527 |
Eurotec® Tecomid® NB40 NL RM PA6, unfilled, MoS2, natural Information provided by Eurotec® |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | ISO 527 |
Eurotec® Tecolen® CP10 GR15 NL PPCP, 15% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | ISO 527-2 |
CENTROPLAST CENTROMID 6 E Polyamide 6 extruded This tough and impact resistant material has good chemical resistance and can be bonded and welded. It is used for sealing rings, flanges, etc. Information provided by CENTROPLAST Engineering Plast.. |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | ASTM D638 |
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness) AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | ISO 527-2 |
CENTROPLAST CENTROMID 6 E FG Polyamide 6 extruded, Food Grade This tough and impact resistant material has good chemical resistance and can be bonded and welded. Information provided by CENTROPLAST Engineering Plastics GMBH |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | ISO 527 |
Eurotec® Tecomid® NB40 MR25 NL IL PA6, 25% mineral reinforced, impact modified, natural Information provided by Eurotec® |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | ISO 527 |
Eurotec® Tecomid® NB40 NL FY50 PA6, unfilled, flame retardant - halogen & red phosphorus free, natural Information provided by Eurotec® |
|||
Tensile Modulus | 3.25 GPa | 471 ksi | |
Radici Radilon® A 42 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |