Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D638 |
Quantum PEI - Ultem® Information provided by Quantum Advanced Engineering Plastics |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | chs 2 in/min; ASTM D638 |
Network Polymers NPS 80-1800 Crystal Polystyrene Description: Injection Molding Grade, High Melt FlowInformation provided by Network Polymers Inc. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ ATH-000/2T Acetal-Homopolymer, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PI-1000 Polyetherimide (PEI)
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D638 |
Fiberfil® PP-60/TC/30 Polypropylene Homopolymer, 30% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D 638 |
Styrolution PS 1600 GPPS Foam extrusion; Injection moldingGood balanced of strength, flow and heat resistanceFree of zinc and oil additivesInformation provided by Styrolution |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D 638 |
Styrolution PS 1900 GPPS Foam extrusionVery high flowHigh heat resistanceFree of zinc and oil additivesInformation provided by Styrolution |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D638 |
Westlake Plastics Tempalux® Polyetherimide For Medical Applications Medical grade Tempalux is made from Ultem® polyetherimide resin, an amorphous thermoplastic which exhibits excellent resistance to a wide range of chemicals and disinfectants. Ultem maintains its .. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D638 |
Total PSC 529 Polystyrene Polystyrene 529 is a medium flow crystal specially formulated for mar resistance. The easy to process crystal minimizes visual defects from ejection and automated part handling. Typical applications.. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D638 |
Total PSC 535 Polystyrene Polystyrene 535 is a high heat crystal polystyrene designed for injection molding, extrusion and blow molding. The material demonstrates excellent strength and good temperature resistance. The varie.. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D638 |
Total PSC 585 Polystyrene Polystyrene 585 is a high molecular weight, low melt flow, crystal polystyrene. This polymer is tailored for extruded foam applications such as egg cartons, meat trays and food service. 585 also mak.. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D638 |
American Polymers API 395 Polystyrene API 395 is one of the highest flowing crystal polystyrenes commercially available. It is produced in pellet form for injection molding and compounding. This material is designed for hard to fill .. |
|||
Tensile Modulus | 2.96 GPa @Temperature 22.8 °C |
430 ksi @Temperature 73.0 °F |
1% Secant; ASTM D638 |
Ensinger Tecapeek® Classix Polyaryletherketone (PAEK) TECAPEEK™ high performance polymer has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's exceptional combination of properties al.. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D638 |
Asahi Kasei Thermylene® P6-10FG-Y950 10% Glass Fiber Reinforced, Lubricated Information provided by Asahi Thermofil |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D638 |
Amco Amalloy® B1044 Polymer Alloy Amco Amalloy B1044 is a proprietary copolymer with exceptional clarity and toughness.Low haze, low melt flow, high tensile & flexural strength.Information provided by Amco Plastic Materials. |