Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.89 GPa | 419 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87160 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C2951 PC+ABS (Asia Pacific) CYCOLOY C2951 is a flame retardant PC+ABS free from chlorinated or brominated flame retardant additives. High heat resistance is offered for demanding electrical applications, whilst maintaining exc.. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP LL004C PEEK LNP* LUBRICOMP* LL004C is a compound based on Polyetheretherketone resin containing 20% PTFE. Added features of this material include: Wear Resistant, Clean Compounding System. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP LL004C PEEK (Asia Pacific) LNP* Lubricomp* LL004C is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated, Clean Compounding System. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP LL004E PEEK LNP* LUBRICOMP* LL004E is a compound based on Polyetheretherketone resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP LL004E PEEK (Asia Pacific) LNP* Lubricomp* LL004E is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM CRS5001 PEI Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM CRS5001 PEI (Asia Pacific) Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM CRS5011 PEI Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM CRS5011 PEI (Asia Pacific) Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DD0009E PC (Asia Pacific) LNP* Stat-kon* DD0009E is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX03571 PC LNP* STAT-KON* DX03571 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS (Europe-Africa-Middle East) Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK (Asia Pacific) LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK (Europe-Africa-Middle East) LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC (Asia Pacific) LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | Neat Resin; ASTM D638 |
Hexcel® HexFlow® RTM 6 180°C Epoxy System for Resin Transfer Molding Monocomponent System HexFlow® RTM 6 is a monocomponent resin already degassed, specifically developed to fulfill the requirements of the aerospace and space industries in advanced resin transfer moulding (RTM) process... |
|||
Tensile Modulus | 2.89 GPa | 419 ksi | ASTM Data |
Americas Styrenics Styron® 612 Polystyrene
(discontinued **) STYRON® 612 general purpose polystyrene resin is an easy flow resin with no color additives. When used unmodified for the manufacture of food contact articles STYRON 612 complies with the US Food, .. |