Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.85 GPa @Thickness 3.20 mm |
414 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: Food Container, Merchandise, Artificial Woods, Refrigerator Vegetable Box, PSP, Sheet, Film, etc.CAS: 9003-53-6-5In.. |