Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.223 GPa @Temperature 50.0 °C |
612.5 ksi @Temperature 122 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |