Polymer Property : Tensile Modulus = 4.06 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.0280 GPa
4.06 ksi
ISO 527-2
Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE)
POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo..
Tensile Modulus 0.0280 GPa
4.06 ksi
ISO 527
Lubrizol ESTANE® GP92AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 92AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Tensile Modulus 0.0280 GPa
4.06 ksi
average; in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® C70.40 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..
Tensile Modulus >= 0.0280 GPa
>= 4.06 ksi
in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® C70.48 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..