Mechanical Properties Metric English Comments
Tensile Modulus 2.64 GPa
383 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP OL009 PPS - Linear
LNP LUBRICOMP* OL009 is a compound based on PPS - Linear resin containing 45% PTFE. Added features of this material include: Wear Resistant.
Tensile Modulus 2.64 GPa
383 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP OL009 PPS - Linear (Asia Pacific)
LNP* LUBRICOMP* OL009 is a compound based on PPS - Linear resin containing PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 2.64 GPa
383 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Asia Pacific)
LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Tensile Modulus 2.64 GPa
383 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Lubricomp XL004 Amorphous Polyamide
LNP* Lubricomp* XL-4040 is a compound based on Amorphous Nylon, containing PTFE.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 2.64 GPa
383 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp YF004 Polyester Elastomer
LNP THERMOCOMP* YF004 is a compound based on Polyester Elastomer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 2.64 GPa
383 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Tensile Modulus 2.64 GPa
383 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Tensile Modulus 2.64 GPa
383 ksi
ISO 527-1
Barlog Plastics KEBAFORM C 25.0 POM Copolymer unreinforced
POMInformation provided by BARLOG plastics GmbH.
Tensile Modulus 2.64 GPa
383 ksi
1mm/min; ISO 527
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Conditioned)
Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla..
Tensile Modulus 2.64 GPa
383 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..