Mechanical Properties Metric English Comments
Tensile Modulus 26.32 GPa
3817 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon EE008E PEI
LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas r..
Tensile Modulus 26.32 GPa
3817 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP JCL36E PES
LNP* LUBRICOMP* JCL36E is a compound based on Polyethersulfone (PES) resin containing 30% Carbon Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.