Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.54 GPa | 368 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2797 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.54 GPa | 368 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |
|||
Tensile Modulus | 2.54 GPa | 368 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Tensile Modulus | 2.54 GPa | 368 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Asia Pacific) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Tensile Modulus | 2.54 GPa | 368 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Tensile Modulus | 2.54 GPa | 368 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT LNP* LUBRICOMP* WI001 is a compound based on PBT containing 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Tensile Modulus | 2.54 GPa | 368 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V2105U PBT Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Tensile Modulus | 2.54 GPa | 368 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY AX06484 ABS LNP* STAT-LOY* AX06484 is a compound based on ABS resin containing Talc. Added feature of this grade is: Antistatic, Extrudeable. |
|||
Tensile Modulus | 2.54 GPa | 368 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-loy AX06484X ABS LNP* Stat-Loy* AX06484 is a compound based on ABS resin containing mineral filler. Characteristics of this grade is it is extrudeable and static dissipative.This data was supplied by SABIC-IP for t.. |
|||
Tensile Modulus | 2.54 GPa | 368 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp 5X06476 FP-V (PVDF) LNP* FP-VM-3830 is a compound based on Polyvinylidine Fluoride (PVDF) containing Mineral.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.54 GPa | 368 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V2105U PBT (Europe-Africa-Middle East) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Tensile Modulus | 2.54 - 2.62 GPa | 368 - 380 ksi | ASTM D638M |
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC +3 DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe.. |
|||
Tensile Modulus | 2.54 - 2.62 GPa | 368 - 380 ksi | ASTM D638M |
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC +3 DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons.. |
|||
Tensile Modulus | 2.54 GPa | 368 ksi | ASTM D-638 |
Axiall 8607 Rigid PVC, Extrusion Georgia Gulf 8607 is a special purpose pelletized compound formulated for high impact, rigid extrusion profiles.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Modulus | 2.54 GPa | 368 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V2105U PBT (Asia Pacific) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Tensile Modulus | 2.53 GPa @Temperature -100 °C |
368 ksi @Temperature -148 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont .. |
|||
Tensile Modulus | 2.54 GPa | 368 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |