Mechanical Properties Metric English Comments
Tensile Modulus 0.250 GPa
36.3 ksi
ISO 527
Premix Thermoplastics PRE-ELEC® ESD 5500 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5500 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5500 can be injectio..
Tensile Modulus 0.250 GPa
36.3 ksi
ISO 527
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injectio..
Tensile Modulus 0.250 GPa

@Temperature 23.0 °C
36.3 ksi

@Temperature 73.4 °F
LATI Lastane 50 PUR
Polyurethane (PUR). Unfilled. Very good noise reduction. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformat..
Tensile Modulus 0.250 GPa
36.3 ksi
ISO 527-1/-2
DSM Arnitel® UM552 Polyether Ester Elastomer (European Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.250 GPa
36.3 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® ELX 40 HNZ TPA
Product description: Grilon ELX 40 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow moulding applications. Grilon ELX 40 H NZ has the follow..
Tensile Modulus 0.250 GPa
36.3 ksi
ISO 527
Eurotec® Tecomid® NB50 NL IT PA6, impact modified, super tough, natural, extrusion grade
Information provided by Eurotec®
Tensile Modulus 0.250 GPa
36.3 ksi
ISO 527-1/-2
DSM Arnitel® UM551-V Polyether Ester Elastomer (European Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.250 GPa
36.3 ksi
ISO 527-1/-2
DSM Arnitel® UM552 55 Shore D Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.250 GPa
36.3 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® L 25 W 40 NZ PA12-I
Product Description: Grilamid L 25 W 40 NZ is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 NZ is impact modified and heat and UV stabilized. The..
Tensile Modulus 0.250 GPa
36.3 ksi
ISO 527-1/-2
DSM Arnitel® UM551-V 55 Shore D, Flame Retardant (halogen-, phosphorous-free) Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.250 GPa
36.3 ksi
Kuraray HYBRAR® PH3 Polypropylene Blend
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber w..
Tensile Modulus 0.250 GPa
36.3 ksi
Henkel SynSpand 9835 Expanding Syntactic Film
Expanding modified epoxy film, cures at 300°F / 149°C, used for jet engine abradable fan seals.