Polymer Property : Tensile Modulus = 338 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.33 GPa
338 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CY6414 PC (Asia Pacific)
Tensile Modulus 2.33 GPa
338 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CY6414 PC (Europe-Africa-Middle East)
Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering high heat for application in appliances, lighting and electrical market.
Tensile Modulus 2.33 GPa
338 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Cycoloy® CY6414 PC+ABS (Europe-Africa-Middle East)
This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Modulus 2.33 GPa
338 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® FXD171R PC
Transparent/transluscent PC for light diffusion special effects. MFR of 25.0.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 2.33 GPa
338 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® FXD171R PC (Asia Pacific)
Transparent/transluscent PC for light diffusion special effects. MFR of 25.0.
Tensile Modulus 2.33 GPa
338 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer
PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp..
Tensile Modulus 2.33 GPa
338 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Asia Pacific)
PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
Tensile Modulus 2.33 GPa
338 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer
ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system.
Tensile Modulus 2.33 GPa
338 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer (Asia Pacific)
ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system.
Tensile Modulus 2.33 GPa
338 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Geloy XTPM309 ASA+PC (Europe-Africa-Middle East)
XTPM309 is a modified HRA170 with improved processing stability.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Modulus 2.33 GPa
338 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Colorcomp DX98735 PC
LNP COLORCOMP* DX98735 is a compound based on Polycarbonate resin containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 2.33 GPa
338 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP COLORCOMP DX98735H PC
LNP* COLORCOMP* DX98735H is an unfilled Polycarbonate resin. Added feature of this grade is: Healthcare.
Tensile Modulus 2.33 GPa
338 ksi
ISO 527-2
Kureha KF Polymer 1000 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Tensile Modulus 2.33 GPa
338 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC
LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Exceptional Processing, Internally Lubricated.
Tensile Modulus 2.33 GPa
338 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC (Asia Pacific)
LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Exceptional Processing.
Tensile Modulus 2.33 GPa
338 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly
LNP* LUBRICOMP* KP002 is a compound based on Acetal Copolymer resin containing 10% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Tensile Modulus 2.33 GPa
338 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KP002 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
Tensile Modulus 2.33 GPa
338 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Xenoy® 1731 PBT+PC
Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.
Tensile Modulus 2.33 GPa

@Thickness 3.20 mm
338 ksi

@Thickness 0.126 in
5 mm/min, Injection Molded; ASTM D638
Styron EMERGEâ„¢ 9500CR Polycarbonate (PC) / Polyethylene Terephthalate (PET)
Overview: EMERGEâ„¢ PC/PET 9500 CR advanced resin is a polycarbonate blend with excellent chemical resistance and ignition resistance properties. This grade was designed for use in medical equipm..
Tensile Modulus 2.33 GPa
338 ksi
ISO 527-2
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by..
Tensile Modulus 2.33 GPa
338 ksi
ISO 527-2
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided ..
Tensile Modulus 2.33 GPa
338 ksi
ISO 527-2
Styron Pulse® 2000EZ PC/ABS
Engineering ResinInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Modulus 2.33 GPa
338 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP 9X11428J PPS
LNP* THERMOCOMP* 9X11428J is a compound based on Polyphenylsulfone containing Proprietary Fillers. Added features of this material include: Healthcare, Low Extractable.
Tensile Modulus 2.33 GPa

@Thickness 4.00 mm
338 ksi

@Thickness 0.157 in
Injection Molded; ISO 527-2
Styron PULSEâ„¢ 2000 EZ PC/ABS Engineering Resin
Overview: PULSE 2000 Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can wi..
Tensile Modulus 2.33 GPa
338 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp..