Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.26 GPa | 328 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® MG34LG ABS Automotive: Low gloss ABS for unpainted interior applications. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Asia Pacific) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXD941A PC (Europe-Africa-Middle East) Transparent/translucent PC for light diffusion special effects. Color package may affect performance. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by .. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by .. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Europe-Africa-Middle East) 7 MFR LEXAN HFD Copolymer |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Asia Pacific) 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Europe-Africa-Middle East) 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer 7 MFR LEXAN HFD Copolymer |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML5472 PC Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | Storage |
Epoxy Technology EPO-TEK® 509FM-1 General Purpose Epoxy Product Description: EPO-TEK® 509FM-1 is a two component, optically opaque epoxy designed for potting of semiconductors, PCB and systems-level electronics. It can be used in many electronic indust.. |
|||
Tensile Modulus | 2.26 GPa | 328 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPH4504H PPC High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |