Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.25 GPa | 327 ksi | IPC 2.4.19 |
Rogers Corporation Ultralam® 3850 Liquid Crystalline Polymer Circuit Material ULTRALAM® 3850 laminate circuit materials utilize highly temperature resistant liquid crystalline polymer (LCP) as the dielectric film.Features & Benefits:Excellent high frequency propertiesStable .. |
|||
Tensile Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
1 mm/min; ASTM D638 |
LG Chemical AF312A ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Tensile Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
1 mm/min; ASTM D638 |
LG Chemical AF360C ABS, TBBA-free Flame Retardant, High Flow Feature: Injection Molding, TBBA-free Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9 and 1309-64-4Information provided by.. |
|||
Tensile Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
LG Chemical HIPS MI770 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HR-1008B PC/ABS, Unreinforced PC/ABS material that can be used for hand phone and car phoneInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NE-1050 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NH-1001T PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced Anti-staticInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® HF-0690M ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0970 MS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0981 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-0927 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HR-1008B PC/ABS, Unreinforced PC/ABS material that can be used for hand phone and car phoneInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NE-1050 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NH-1001T PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced Anti-staticInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® HF-0690M ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0970 MS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0981 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-0927 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.26 GPa | 327 ksi | Storage |
Epoxy Technology EPO-TEK® 301 Spectrally Transparent Epoxy Product Description: EPO-TEK® 301 is a two component, room temperature curing epoxy featuring very low viscosity, and excellent optical-mechanical properties.Advantages & Application Notes: Semicon.. |