Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 221 GPa | 32100 ksi | |
Zoltek Panex 30® High Twist Carbon Roving High Twist Carbon RovingApplications include: Friction Clutches & Brakes, Composite Substructures |
|||
Tensile Modulus | 221 GPa | 32100 ksi | |
Goodfellow Evanohm® Precision Resistance Nickel Alloy Electrical resistance alloy with a very low temperature coefficient of resistivityInformation provided by Goodfellow. |
|||
Tensile Modulus | 221 GPa | 32100 ksi | Typical fiber property; Chord 6000-1000 |
Hexcel® HexTow™ AS2C Carbon Fiber HexTow™ AS2C carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 3,000 (3K), 6,000 (6K), and 12,000 (12K) filament count tows. This fiber has been surface treated.. |