Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.15 GPa @Thickness 3.20 mm |
311 ksi @Thickness 0.126 in |
1 mm/min; ASTM D638 |
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Modulus | 2.15 GPa @Thickness 3.20 mm |
311 ksi @Thickness 0.126 in |
1 mm/min; ASTM D638 |
LG Chemical HF380U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Modulus | 2.15 GPa @Thickness 3.20 mm |
311 ksi @Thickness 0.126 in |
1 mm/min; ASTM D638 |
LG Chemical HF350U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Modulus | 2.15 GPa @Thickness 3.20 mm |
311 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |