Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.12 GPa
307 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer
Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h..
Tensile Modulus 2.12 GPa
307 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Asia Pacific)
Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h..
Tensile Modulus 2.12 GPa
307 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h..
Tensile Modulus 2.12 GPa
307 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer
11 MFR LEXAN High Flow Ductile Copolymer
Tensile Modulus 2.12 GPa
307 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Asia Pacific)
11 MFR LEXAN High Flow Ductile Copolymer
Tensile Modulus 2.12 GPa
307 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP AI001XXH ABS
LNP* Lubricomp* AI001XXH is a compound based on ABS containing 2% Silicone. Characteristics of this grade are: Healthcare and Internally Lubricated.
Tensile Modulus 2.12 GPa
307 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® EXRL0683 PC Copolymer
11 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 2.12 GPa
307 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Europe-Africa-Middle East)
11 MFR LEXAN High Flow Ductile Copolymer
Tensile Modulus 2.12 GPa
307 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer
11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only
Tensile Modulus 2.12 GPa
307 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Asia Pacific)
11 MFR LEXAN High Flow Ductile Copolymer UV stabilized
Tensile Modulus 2.12 GPa
307 ksi
ISO 527-2
Kureha KF Polymer 2950 PVDF Copolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Tensile Modulus 2.12 GPa
307 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DP0039EF PC (Asia Pacific)
LNP* Lubricomp* DP0039EF is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 2.12 GPa
307 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRILOY D20001 PPO
LNP* LUBRILOY* Z20001 is a compound based on PPO resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant.
Tensile Modulus 2.12 GPa
307 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON CD0001 PS
LNP* STAT-KON* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Tensile Modulus 2.12 GPa
307 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON CD000I PS
LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Tensile Modulus 2.12 GPa
307 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP 67002XXH PBT+PC
LNP* THERMOCOMP* 67002XXH is a compound based on PBT+PC containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added features inc..
Tensile Modulus 2.12 GPa
307 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 POLYPHENYLENESULFONE (Asia Pacific)
LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral.
Tensile Modulus 2.12 GPa
307 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 PPS
LNP* THERMOCOMP* 9X04488 is a compound based on PPS resin containing Mineral.
Tensile Modulus 2.12 GPa
307 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL PKN4775 PPE+PS
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
Tensile Modulus 2.12 GPa
307 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL PKN4775 PPE+PS
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
Tensile Modulus 2.12 GPa
307 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Asia Pacific)
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
Tensile Modulus 2.12 GPa
307 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Asia Pacific)
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
Tensile Modulus 2.12 GPa
307 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Europe-Africa-Middle East)
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
Tensile Modulus 2.12 GPa
307 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Europe-Africa-Middle East)
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
Tensile Modulus 2.12 GPa
307 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66
LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Tensile Modulus 2.12 GPa
307 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp 9X04488 POLYPHENYLENESULFONE
LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 2.12 GPa
307 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Europe-Africa-Middle East)
11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only
Tensile Modulus 2.12 GPa
307 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRILOY Z20001 PPO
LNP* Lubriloy* Z20001 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant.