Polymer Property : Tensile Modulus = 3.63 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.63 GPa
526 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP KAL22 Acetal Copolymer
LNP* LUBRICOMP* KAL22 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Fiber. Added feature of this material is: Wear Resistant.
Tensile Modulus 3.63 GPa
526 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP KZ002 Acetal
LNP* THERMOCOMP* KZ002 is a compound based on Acetal containing 10% Milled Glass.
Tensile Modulus 3.63 GPa
526 ksi
Storage
Epoxy Technology EPO-TEK® 320-3 Optically Opaque Epoxy
Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific..