Polymer Property : Tensile Modulus = 3.61 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.61 GPa
524 ksi
ASTM D882
NatureWorks® Ingeo™ 2003D General Purpose Transparent Extrusion Grade Biopolymer
NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. PLA polymer 2003D processes easily on conventional extrusion equipment. Specifically designed fo..
Tensile Modulus 3.61 GPa
524 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP MX88028 PP
LNP* THERMOCOMP* MX88028 is a compound based on Polypropylene resin containing Proprietary Filler(s).
Tensile Modulus 3.61 GPa
524 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP MX88028 PP (Asia Pacific)
LNP* Thermocomp* MX88028 is a compound based on Polypropylene resin containing Glass Fiber.