Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.53 GPa | 512 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA LNP* LUBRILOY* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 3.53 GPa | 512 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA (Asia Pacific) LNP* Lubriloy* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 3.53 GPa | 512 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled Material with 10% GF reinforcement with high stiffness that can be used in refrigerator vegetable boxesInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 3.53 GPa | 512 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled Material with 10% GF reinforcement with high stiffness that can be used in refrigerator vegetable boxesInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 3.53 GPa @Temperature -70.0 °C |
511 ksi @Temperature -94.0 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Modulus | 3.53 GPa @Temperature 80.0 °C |
512 ksi @Temperature 176 °F |
ISO Data |
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin.. |
|||
Tensile Modulus | 3.53 GPa | 512 ksi | same value from ASTM and ISO test. |
BASF Capron® GR20 20% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR20 is a 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also.. |
|||
Tensile Modulus | 3.53 GPa | 512 ksi | same value from ASTM and ISO test. |
BASF Capron® GR20 HS 20% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR20 HS is a heat stabilized 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |