Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.48 GPa | 505 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON KX02764 Acetal LNP STAT-KON* KX02764 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 3.48 GPa | 505 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl PX0346 PPE+PS This data was supplied by SABIC-IP for the Americas region. |