Mechanical Properties Metric English Comments
Tensile Modulus 3.25 GPa
471 ksi
Plastcom SLOVALEN PH 99 GB 30 LS PP, 30% glass beads, mod. of mech. properties
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP...
Tensile Modulus 3.25 GPa
471 ksi
Type 1B, 50mm/min; ISO 527-1/2:1993
Nylacast Impact Nylon 6, Impact Grade
Nylacast Impact has been designed for applications that have a high impact resistance and noise reduction capabilities. It works more effectively in applications where there are high stress. It also..
Tensile Modulus 3.25 GPa
471 ksi
1 mm/min; ISO 527
Polimeri Europa Edistir N 1782 Polystyrene
General purpose polystyrene with good flow and high heat resistance. Suggested for direct gassing extrusion of heavy gage insulating boards (XPS) and in blend with high concentration of clear SBS f..
Tensile Modulus 3.25 GPa
471 ksi
1 mm/min; ISO 527
Polimeri Europa Edistir N 1840 Polystyrene
General purpose polystyrene combining easy flow and medium heat. Edistir N 1840 is suggested in extrusion for glossy capping of HIPS sheets and for blending with HIPS or clear SBS for stiffer therm..
Tensile Modulus 3.25 GPa
471 ksi
1 mm/min; ISO 527
Polimeri Europa Edistir N 2560 Polystyrene
High molecular weight general purpose polystyrene with good mechanical strength and good thermal resistance. It is recommended for in-line forming of disposable packaging, for sheet extrusion in ble..
Tensile Modulus 3.25 GPa
471 ksi
ISO 527-1/2
Radici Radilon® ALX14080 (dry) Nylon 66
Medium high viscosityInformation provided by Radici group.
Tensile Modulus 3.25 GPa
471 ksi
1 mm/min
Polimeri Europa EDISTIR N1460 Polystyrene  (discontinued **)
Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,E,085-03 High molecular weight general purpose polystyrene with good mechanical strength. This grade is especially recomme..
Tensile Modulus 3.25 GPa
471 ksi
1 mm/min
Polimeri Europa EDISTIR N1461 Polystyrene  (discontinued **)
Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,085-03 High molecular weight general purpose polystyrene with good mechanical strength. Well suitable for injection mold..
Tensile Modulus 3.25 GPa
471 ksi
1 mm/min
Polimeri Europa EDISTIR N1841 Polystyrene  (discontinued **)
Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,085-12 General purpose polystyrene combining easy flow and medium heat. This grade exhibits excellent processability in ..
Tensile Modulus 3.25 GPa
471 ksi
ISO 527
FKuR Kunststoff Fibrolon® P 7550 Wood-Plastic Compound, Fiber Reinforced
FIBROLON® are fiber reinforced compounds. Fibrolon® P 7550 has a polypropylene base. With the brand name of FIBROLON® FKuR has developed natural fiber reinforced compounds (Wood-Plastics-C..
Tensile Modulus 3.25 GPa

@Temperature 80.0 °C
471 ksi

@Temperature 176 °F
1 mm/min; ISO 527
SABIC Innovative Plastics SABIC STAMAX 20YK270 PP
SABIC® STAMAX 20YK270 is a 20% long glass fiber reinforced polypropylene with improved impact and flow properties. The glass fibers are chemically coupled to the PP matrix, resulting in high stif..
Tensile Modulus 3.25 GPa
471 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP EX00781H PEI
LNP* THERMOCOMP* EX00781H is a compoud based on Polyetherimide containng Proprietary Filler(s). Added feature of this material is: Healthcare.
Tensile Modulus 3.25 GPa
471 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP MFB22S PP
LNP* THERMOCOMP* MFB22S is a compound based on Polypropylene containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Heat Stabilized.
Tensile Modulus 3.25 GPa
471 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66
Conductive GTX, CTE 7
Tensile Modulus 3.25 GPa
471 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 (Asia Pacific)
Conductive GTX, CTE 7
Tensile Modulus 3.25 GPa
471 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 (Europe-Africa-Middle East)
Conductive GTX, CTE 7
Tensile Modulus 3.25 GPa
471 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP
LNP THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Modulus 3.25 GPa

@Temperature 22.8 °C
471 ksi

@Temperature 73.0 °F
ASTM D638
Ensinger TECANYL™ MT Autoclavable Polymer
TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease..
Tensile Modulus 3.25 GPa

@Temperature 22.8 °C
471 ksi

@Temperature 73.0 °F
ASTM D638
Ensinger TECANYL™ MT XRO Autoclavable Polymer
TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease..
Tensile Modulus 3.25 GPa
471 ksi
ISO 527
Eurotec® Tecomid® NA40 MR15 NL IL PA6.6, 15% mineral filled, impact modified, natural
Information provided by Eurotec®
Tensile Modulus 3.25 GPa
471 ksi
ISO 527
Eurotec® Tecomid® NB40 NL FY70 PA6, flame retardant - halogen free (RoHS compliant), natural
Information provided by Eurotec®
Tensile Modulus 3.25 GPa
471 ksi
ISO 527
Eurotec® Tecomid® NB40 NL RM PA6, unfilled, MoS2, natural
Information provided by Eurotec®
Tensile Modulus 3.25 GPa
471 ksi
ISO 527-1/-2
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..
Tensile Modulus 3.25 GPa
471 ksi
ISO 527
Eurotec® Tecolen® CP10 GR15 NL PPCP, 15% glass fiber reinforced, natural
Information provided by Eurotec®
Tensile Modulus 3.25 GPa
471 ksi
ISO 527-2
CENTROPLAST CENTROMID 6 E Polyamide 6 extruded
This tough and impact resistant material has good chemical resistance and can be bonded and welded. It is used for sealing rings, flanges, etc. Information provided by CENTROPLAST Engineering Plast..
Tensile Modulus 3.25 GPa
471 ksi
ASTM D638
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness)
AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Tensile Modulus 3.25 GPa
471 ksi
ISO 527-2
CENTROPLAST CENTROMID 6 E FG Polyamide 6 extruded, Food Grade
This tough and impact resistant material has good chemical resistance and can be bonded and welded. Information provided by CENTROPLAST Engineering Plastics GMBH
Tensile Modulus 3.25 GPa
471 ksi
ISO 527
Eurotec® Tecomid® NB40 MR25 NL IL PA6, 25% mineral reinforced, impact modified, natural
Information provided by Eurotec®
Tensile Modulus 3.25 GPa
471 ksi
ISO 527
Eurotec® Tecomid® NB40 NL FY50 PA6, unfilled, flame retardant - halogen & red phosphorus free, natural
Information provided by Eurotec®
Tensile Modulus 3.25 GPa
471 ksi
Radici Radilon® A 42 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..