Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.19 GPa | 462 ksi | MD; ASTM D638 |
Rogers Corporation RO3206 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Tensile Modulus | 3.19 GPa | 462 ksi | TD; ASTM D638 |
Rogers Corporation RO3206 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Tensile Modulus | 3.19 GPa | 463 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DZL24 PC LNP LUBRICOMP* DZL24 is a compound based on Polycarbonate resin containing 20% Milled Glass, 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 3.19 GPa | 463 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Asia Pacific) Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Tensile Modulus | 3.19 GPa | 463 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Europe-Africa-Middle East) Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Tensile Modulus | 3.19 GPa | 463 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |