Polymer Property : Tensile Modulus = 3.18 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.18 GPa
461 ksi
ASTM D638
Greene Tweed ARâ„¢ HT Abrasive-Resistant Thermoplastic
ARHT™ is a proprietary thermoplastic material specifically developed for use a sbushings, bearings and wear rings in pumps handling abrasive media up to 250°F (121°C). ARHT provides outs..
Tensile Modulus 3.18 GPa
461 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP EX03599H PEI
LNP* LUBRICOMP* EX03599H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant.
Tensile Modulus 3.18 GPa
461 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer
LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant.
Tensile Modulus 3.18 GPa
461 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Asia Pacific)
LNP* Lubricomp* KG002 is a compound based on Acetal Copolymer resin containing Graphite Powder. Added features of this material include: Internally Lubricated.
Tensile Modulus 3.18 GPa
461 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RX99518 PA 66
LNP* LUBRICOMP* RX99518 is a compound based on PA66 containing Proprietary Fillers. Added feature of this material is: Wear Resistant.
Tensile Modulus 3.18 GPa
461 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP AX06437 ABS
LNP* THERMOCOMP* AX06437 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable.
Tensile Modulus 3.18 GPa
461 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP AX08306 ABS
LNP* THERMOCOMP* AX08306 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable.
Tensile Modulus 3.18 GPa
461 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP AX08306 ABS (Asia Pacific)
LNP* Thermocomp* AX08306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Mineral.
Tensile Modulus 3.18 GPa
461 ksi
Storage
Epoxy Technology EPO-TEK® OE120 Two Component Epoxy
Material Description: A two component, opaque epoxy, designed for fiber optics packaging applications. It is a black-colored version of EPO-TEK 353ND-T. It has a high Tg for resisting elevated ope..