Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D638 |
PolyOne Nymax™ 604 NU Natural Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Tensile Modulus | 3.17 GPa @Thickness 6.40 mm |
460 ksi @Thickness 0.252 in |
ASTM D638 |
SABIC Innovative Plastics Lexan® FL910 PC Various weight reductions at 0.250"" (6.35 mm) wall, 10% GR. High flexural strength and modulus, impact/heat resistant. V-0/5V at 0.250"" (6.35 mm). |
|||
Tensile Modulus | 3.17 GPa @Thickness 6.40 mm |
460 ksi @Thickness 0.252 in |
ASTM D638 |
SABIC Innovative Plastics Lexan® FL913 PC Various weight reduction at 0.250"" (6.35 mm) wall. 10% GR, high flexural strength/modulus. UL rated V-0/5VA (all except natural). UV-stabilized. |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM Data |
Americas Styrenics Styron® 663 Polystyrene
(discontinued **) STYRON® 663 general purpose polystyrene resin is an additive free resin with excellent strength, clarity, and high heat resistance. When used unmodified for the manufacture of food contact articles.. |
|||
Tensile Modulus | 3.17 GPa @Thickness 6.40 mm |
460 ksi @Thickness 0.252 in |
ASTM D638 |
SABIC Innovative Plastics Lexan® FL410 PC Various weight reductions at 0.250: (6.38 mm) wall. Thin wall capability high flexural mod, strength and creep resistant. V-0/5V - 0.157""(3.98 mm). |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D638 |
M. Holland Company GS230WC Polystyrene, Specialty High clarityCrystallineHigh heat resistanceGood mold releaseApplications: BottlesLabwareVials |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RL002 PA 66 LNP LUBRICOMP* RL002 is a compound based on Nylon 66 resin containing 10% PTFE. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp RL0049 PA 66 LNP* Lubricomp* RL0049 is a compound based on Nylon 66 resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant.This data was supplied.. |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RL0049S PA 66 LNP LUBRICOMP* RL0049S is a compound based on Nylon 66 resin containing 20% PTFE. Added features of this material include: Flame Retardant, Heat Stabilized, Wear Resistant. |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D 638 |
Styrolution PS 1200/1201 GPPS Extrusion / thermoforming foam sheetHigh melt strengthHigh StiffnessUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D 638 |
Styrolution PS 1290/1291 GPPS Extrusion / thermoforming foam sheetLow residual styrene monomer contentHigh melt strength and stiffnessUL Classification 94 HB for 1290Information provided by Styrolution |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D 638 |
Styrolution PS 1621 GPPS Easy flow material with excellent moldabilityExcellent clarity and set-up timeInformation provided by Styrolution |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D 638 |
Styrolution PS 2600/2601 GPPS Foam extrusionLow residual styrene monomer contentModerate heat resistanceGood balance of strength and ease of processingUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolut.. |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D 638 |
Styrolution PS 3100/3101 GPPS Good balance of flow and set-up propertiesModerate heat resistanceUSP Class VI certifiedInformation provided by Styrolution |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D 638 |
Styrolution PS 3190/3191 GPPS Low residual styrene monomer contentGood balance of flow and set-up propertiesInformation provided by Styrolution |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D 638 |
Styrolution PS 3600/3601 GPPS Exceptional flow characteristicsGood for thin wall and complex partsUSP Class VI certifiedInformation provided by Styrolution |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON RD000 PA 66 LNP STAT-KON* RD000 is a compound based on Nylon 66 resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D 638 |
Styrolution PS 2610 GPPS Extruded packaging; Thermoforming applicationsExcellent toughnessHigh melt strengthGood flow and processabilityInformation provided by Styrolution |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ISO 527 |
Ecomass® 1007ZC85 Stainless Steel Filled COPA Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsStainless Steel Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by Technical Poly.. |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D638 |
Ecomass® 3800ZD82 Tungsten Filled Polymethylpentene Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polymethylpentene (TPX)RigidInformation provided by Technical Polymers |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | 0.2 in/min; 0.125" thickness; ASTM D-638 |
Chevron Phillips MB3150 Crystal Polystyrene High heat crystal polystyrene.Applications:Compact disc jewel boxesConsumer containers, vials, jars, etc.Desk organizersAudio cassettesFeatures:Fast cycling due to high heat distortionHigh Vicat sof.. |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D638 |
Cast Nylons Nycast® SLX Premium Bearing Grade Nylon Nycast® SLX closes the gap between static and dynamic coefficients of friction. Used in wear pads, bearing blocks, and other load-bearing slide applications.Data provided by the manufacturer, Cast.. |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D638 |
Americas Styrenics MC3650 High Heat Crystal Polystyrene Product CharacteristicsImproved cycle times in hard to fill partsExcellent clarity with slight blue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsHousewaresConsumer.. |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D638 |
Americas Styrenics STYRON® 666D High Heat Crystal Polystyrene Product CharacteristicsMedium heat resistanceMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsMedicalPackaging/disposablesInformation provided by AmericasStyrenics LLC. |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D638 |
Americas Styrenics STYRON® 668 High Heat Crystal Polystyrene Product CharacteristicsHigh heatGood balance of flow and toughnessFood Contact CompliantUL Classification 94HBTypical ApplicationsDisposable cutleryCD and DVD jewel boxesInformation provided by Amer.. |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D638 |
Americas Styrenics STYRON® 675 High Heat Crystal Polystyrene Product CharacteristicsHigh heatMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsThin-walled partsInformation provided by AmericasStyrenics LLC. |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D638 |
Americas Styrenics STYRON® 685D High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthBlue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsFoamOPSMedicalInformation provided by AmericasSty.. |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D638 |
Americas Styrenics STYRON® 685DL High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthBlue tintFood Contact CompliantTypical ApplicationsFoamOPSMedicalInformation provided by AmericasStyrenics LLC. |
|||
Tensile Modulus | 3.17 GPa | 460 ksi | ASTM D638 |
Americas Styrenics STYRON® 695 High Heat Crystal Polystyrene Product CharacteristicsReduced residualsHigh heat resistancehigh strengthFood Contact CompliantTypical ApplicationsOPSInformation provided by AmericasStyrenics LLC. |