Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 3.10 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.76 - 3.10 GPa
400 - 450 ksi
ASTM D790
Alcoa KAMA 2100 Prime Clear OPS, Film  (discontinued **)
CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti..
Tensile Modulus 2.76 - 3.10 GPa
400 - 450 ksi
ASTM D790
Alcoa KAMA 2200 Prime Graphic Arts OPS  (discontinued **)
CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti..
Tensile Modulus 2.76 - 3.10 GPa
400 - 450 ksi
ASTM D790
Alcoa KAMA 2600 Envelope Window, Film  (discontinued **)
CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti..
Tensile Modulus 2.76 - 3.10 GPa
400 - 450 ksi
ASTM D790
Alcoa KAMA 2700 OPS Lamination, Film  (discontinued **)
CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti..
Tensile Modulus 1.70 - 3.10 GPa
247 - 450 ksi
ASTM D638
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Tensile Modulus 2.76 - 3.10 GPa
400 - 450 ksi
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting
Product Description: Master Bond EP17HT is an one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation prof..
Tensile Modulus 2.76 - 3.10 GPa
400 - 450 ksi
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting
Product Description: Master Bond EP17HT-LO is a one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation pr..
Tensile Modulus 2.70 - 3.10 GPa
392 - 450 ksi
Dow CYCLOTENE™ 3022-35 Bisbenzocyclobutene (BCB) Electronic Resin
This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow
Tensile Modulus 2.70 - 3.10 GPa
392 - 450 ksi
Dow CYCLOTENE™ 3022-46 Bisbenzocyclobutene (BCB) Electronic Resin
This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow
Tensile Modulus 2.70 - 3.10 GPa
392 - 450 ksi
Dow CYCLOTENE™ 3022-57 Bisbenzocyclobutene (BCB) Electronic Resin
This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow
Tensile Modulus 2.70 - 3.10 GPa
392 - 450 ksi
Dow CYCLOTENE™ 3022-63 Bisbenzocyclobutene (BCB) Electronic Resin
This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow
Tensile Modulus 2.70 - 3.10 GPa
392 - 450 ksi
Dow CYCLOTENE™ 4022-35 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ 4022-35 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Modulus 2.70 - 3.10 GPa
392 - 450 ksi
Dow CYCLOTENE™ 4024-40 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ 4024-40 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Modulus 2.70 - 3.10 GPa
392 - 450 ksi
Dow CYCLOTENE™ 4026-46 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ 4026-46 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Modulus 2.70 - 3.10 GPa
392 - 450 ksi
Dow CYCLOTENE™ XU35075 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ XU35075 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Modulus 2.70 - 3.10 GPa
392 - 450 ksi
Dow CYCLOTENE™ XU35132 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ XU35132 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Modulus 2.70 - 3.10 GPa
392 - 450 ksi
Dow CYCLOTENE™ XU35133 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ XU35133 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Modulus 2.69 - 3.10 GPa
390 - 450 ksi
ASTM D638
3D Systems Accura® 60 Plastic for SLA® Systems
Simulate the properties and appearance of polycarbonate. For use with solid-state stereolithography (SLA®) systems.ApplicationsTough functional prototypesAutomotive design componentsConsumer electr..
Tensile Modulus 2.76 - 3.10 GPa
400 - 450 ksi
ASTM D790
Alcoa KAMA 1120 Prime AntiFog OPS, Sheet  (discontinued **)
CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati..
Tensile Modulus 2.76 - 3.10 GPa
400 - 450 ksi
ASTM D790
Alcoa KAMA 1200 Utility Clear OPS, Sheet  (discontinued **)
CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati..
Tensile Modulus 2.76 - 3.10 GPa
400 - 450 ksi
ASTM D790
Alcoa KAMA 1100 Prime Clear OPS, Sheet  (discontinued **)
CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati..
Tensile Modulus 2.69 - 3.10 GPa
390 - 450 ksi
ASTM D638
Proto3000 Accura® 60 Plastic Stereolithography (SLA) Prototyping Polymer
Features:Durable and stiffHigh clarityFast build speedLow viscosity formulationHumidity resistant partsFully developed and tested build stylesBenefits:Achieve the look and feel of polycarbonateView ..
Copyright © lookpolymers.com All Rights Reserved