Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.07 GPa
445 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Dry Blend E7009 Polyvinyl Chloride, Rigid (PVC, Rigid)
Recommended for whites and light pastel colors only. Not to be used for darker colors.Physical properties based on Geon E7009 white 1024 lot# UTCX 57572Information provided by PolyOne
Tensile Modulus 3.07 GPa
445 ksi
ASTM D638
M. Holland Company GS411 Polystyrene  (discontinued **)
Features: Good Crack Resistance, Crystal, Fast Cycle (Production), Good FlowUses: Disposable Drinkware, Electrical/Electronic ApplicationsApprovals: FDA 21 CFR 177.1640 Processing Method: Extrusio..
Tensile Modulus 3.07 GPa
445 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP LL003 PEEK
LNP* LUBRICOMP* LL003 is a compond based on Polyetheretherketone resin containing 15% PTFE Lubricant. Added feature of this material is: Wear Resistant.
Tensile Modulus 3.07 GPa
445 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON IS000XXL PA6.12
LNP* STAT-KON* IS000XXL is a compound based on Nylon 6/12 containing Stainless Steel Fibers. Added features of this material include: Food Contact Compliant Raw Materials, Metal Detectable, Electr..
Tensile Modulus 3.07 GPa
445 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp YF006 TPEE
LNP THERMOCOMP* YF006 is a compound based on TPEE resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 3.07 GPa
445 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Lubricomp LL003E PEEK
LNP* Lubricomp* LL003E is a compound based on Polyetheretherketone (PEEK) containing PTFE. Characteristics of this grade are: Easy Molding and Internally Lubricated.This data was supplied by SABIC..
Tensile Modulus 3.07 GPa
445 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon IS000LX PA6.12
LNP* Stat-Kon* IS000LX is a compound based on Nylon 6/12 containing Stainless Steel Fibers.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 3.07 GPa
445 ksi
ASTM D638
Americas Styrenics STYRON® 686E High Heat Crystal Polystyrene
Product CharacteristicsExceptional balance between heat resistance, toughness and flowGood dimensional stability and excellent clarityFood Contact CompliantTypical ApplicationsFoamed PS sheets used ..
Tensile Modulus 3.07 GPa
445 ksi
Abatron AboCast 8103-20 High-Performance Dielectric Epoxy
AboCast 8103-20 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system is unique ..