Polymer Property : Tensile Modulus = 292 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.01 GPa
292 ksi
5.1 mm/min; ASTM D638
PolyOne Geon™ L4605 Ivory 3098 Polyvinyl Chloride, Semi-Rigid (PVC, Semi-Rigid)
Information provided by PolyOne
Tensile Modulus 2.01 GPa
292 ksi
ASTM D638
Eastman Eastar GN125 Copolyester, Natural  (discontinued **)
Eastar Copolyester GN125 is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet light inhibitor. This product is recommended for indoor applications requiring enhanced co..
Tensile Modulus 2.01 GPa
292 ksi
1mm/min
Eastman Tenite 105-28 Cellulose Acetate  (discontinued **)
28% Plasticized ISO data as provided by the manufacturer, Eastman Chemical.
Tensile Modulus 2.01 GPa
292 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC
LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Easy Molding, Internally Lubricated, Healthcare.
Tensile Modulus 2.01 GPa
292 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics SABIC PPCOMPOUND 7705 PP
SABIC® PPcompound 7705 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, scratch resistance, and heat stability with interior automotive UV stabili..
Tensile Modulus 2.01 GPa
292 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific)
PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability
Tensile Modulus 2.01 GPa
292 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS
LNP STAT-LOY* A3000 is a compound based on ABS resin. Added feature of this material is: Antistatic.
Tensile Modulus 2.01 GPa
292 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Asia Pacific)
LNP STAT-LOY A3000 is a compound based on Acrylonitrile butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistatic. Also known as: STAT-LOY A
Tensile Modulus 2.01 GPa
292 ksi
ASTM D638
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Tensile Modulus 2.01 GPa
292 ksi
ASTM D638
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Tensile Modulus 2.01 GPa
292 ksi
1mm/min
Eastman Eastar DN003 PCTG Copolyester
ISO data as provided by the manufacturer, Eastman Chemical
Tensile Modulus 2.01 GPa

@Temperature -50.0 °C
292 ksi

@Temperature -58.0 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm..